Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Europe - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 12 cm³/10min ISO 1133
温度 260 °C -
荷重 5 kg -
溶融時の熱伝導率 0.21 W/(m K) -
溶融時の比熱 2300 J/(kg K) -
突き出し時の時の温度 142 °C -
機械的特性単位テスト基準
ISO データ
引張弾性率 1370 MPa ISO 527
降伏応力 35 MPa ISO 527
降伏ひずみ 5 % ISO 527
破壊応力 31 MPa ISO 527
破壊ひずみ 50 % ISO 527
曲げ弾性率 1520 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30゚C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 37 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 6 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
ノッチ付きアイゾット衝撃強さ, +23°C, 4mm 36 kJ/m² ISO 180/1A
ノッチ付きアイゾット衝撃強さ, -30°C, 4mm 10 kJ/m² ISO 180/1A
ロックウェル硬度 R 60 - ISO 2039-2
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, B 80 °C ISO 306
ビカット軟化温度, 120°C/h 50N 85 °C ISO 306
線膨張係数, 平行 70.7 E-6/K ISO 11359-1/-2
線膨張係数, 直角 101 E-6/K ISO 11359-1/-2
その他の特性.単位テスト基準
密度. 990 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 60 - 65 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
樹脂温度 260 - 290 °C -
金型温度 40 - 60 °C -
Feed temperature 60 - 80 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 285 °C -
Zone 3 250 - 290 °C -
機能
 粘度せん断速度. , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
 せん断応力-せん断速度. , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
 pvT , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
特殊な特性
成形加工法.
射出成形.
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.